Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 350000 - 450000 cP @Temperature 25.0 °C |
350000 - 450000 cP @Temperature 77.0 °F |
|
Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes EPOCYL™ NC E128-02 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enh.. |
|||
Viscosity | 350000 - 450000 cP @Temperature 25.0 °C |
350000 - 450000 cP @Temperature 77.0 °F |
|
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6 EPOCYL™ NC R128-02 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of.. |
|||
Viscosity | 350000 - 550000 cP | 350000 - 550000 cP | Paste |
ND Industries 460 Instant High Pressure Pipe Sealant High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings |
|||
Viscosity | 350000 cP @Temperature 200 °C |
350000 cP @Temperature 392 °F |
melt; 1000 sec-1; ASTM D 3825 |
SABIC Innovative Plastics Cycolac® FR30U ABS Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Viscosity | 350000 cP | 350000 cP | Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
Viscosity | 350000 cP @Temperature 400 °C |
350000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Viscosity | 350000 cP @Temperature 400 °C |
350000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
Viscosity | 350000 cP @Temperature 400 °C |
350000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Viscosity | 350000 cP @Temperature 400 °C |
350000 cP @Temperature 752 °F |
ISO 11443 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Viscosity | 350000 cP @Temperature 400 °C |
350000 cP @Temperature 752 °F |
ISO 11443 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Viscosity | 350000 - 600000 cP @Temperature 220 - 220 °C |
350000 - 600000 cP @Temperature 428 - 428 °F |
Average value: 475000 cP Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Viscosity | 350000 cP | 350000 cP | |
Loctite® PST® 592 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 350000 - 550000 cP | 350000 - 550000 cP | Dynamic |
Dow Corning 9045 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, suncare, shower gel, hair care, and color cosmetic applications.Informati.. |
|||
Viscosity | 350000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
350000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 350000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F132-E2 PA6 High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 350000 cP @Temperature 160 °C |
350000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 350000 - 550000 cP @Temperature 23.0 °C |
350000 - 550000 cP @Temperature 73.4 °F |
0.5 rpm |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Viscosity | 350000 cP @Shear Rate 300 1/s, Temperature 190 °C |
350000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 350000 cP @Temperature 25.0 °C |
350000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 224-8 Room Temperature Cure Epoxy Adhesive TRA-BOND 224-8 room temperature cure epoxy adhesive is a thermally conductive version of 224-1. This adhesive develops structural strength rapidly. When cured at room temperature, this adhesive prov.. |
|||
Viscosity | 350000 - 850000 cP @Temperature 400 - 400 °C |
350000 - 850000 cP @Temperature 752 - 752 °F |
Average value: 445000 cP Grade Count:3 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Viscosity | 350000 - 700000 cP | 350000 - 700000 cP | |
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4.. |
|||
Viscosity | 350000 cP @Temperature 400 °C |
350000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |