Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 210000 cP | 210000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Viscosity | 210000 cP | 210000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Viscosity | 210000 cP | 210000 cP | Melt Viscosity, 250°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Viscosity | 210000 cP | 210000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Viscosity | 210000 cP | 210000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Viscosity | 210000 cP | 210000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Viscosity | 210000 cP @Temperature 25.0 °C |
210000 cP @Temperature 77.0 °F |
Mixed (cp #52, 2.5 rpm) |
Tra-Con Tra-Bond 789-3T3N1 Moisture Resistant Adhesive TRA-BOND 789-3T3N1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistan.. |
|||
Viscosity | 210000 cP | 210000 cP | dynamic |
Dow Corning HM-2500 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Viscosity | 210000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
210000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® FR3010 IF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Viscosity | 210000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
210000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Viscosity | 210000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
210000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Viscosity | 210000 cP @Temperature 250 °C |
210000 cP @Temperature 482 °F |
DAM; @ 1000 sec-1; ISO 11443 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Viscosity | 210000 cP | 210000 cP | Mixed |
Armstrong A-2/A Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |