Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 15000 cP | 15000 cP | |
NextGen Adhesives M907-11 Medical Grade Epoxy Adhesive Description: NGAC M907-11 is a medium viscosity adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include laminating, bonding.. |
|||
Viscosity | 15000 - 30000 cP @Temperature 25.0 °C |
15000 - 30000 cP @Temperature 77.0 °F |
Uncured |
Permabond ES562 Epoxy Resin PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t.. |
|||
Viscosity | 15000 - 25000 cP @Temperature 40.0 °C |
15000 - 25000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 15000 cP | 15000 cP | |
Shin-Etsu Silicones KE-441 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 15000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
15000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-85-1000 TPE Product Description: StarXTRUDE XTR-85-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |
|||
Viscosity | 15000 - 60000 cP | 15000 - 60000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U0251M Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | <= 15000 cP | <= 15000 cP | #3 SP @ 12 rpm; RP-0596 |
Solvay MIRASHEEN® CP-820 Surfactant Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related produ.. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | Part A |
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance.. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 15 LV Variable Hardness Low Viscosity Catalyst Emerson & Cuming 15 LV Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. .. |
|||
Viscosity | 15000 cP | 15000 cP | Part B |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Viscosity | 15000 - 30000 cP | 15000 - 30000 cP | Part A |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 3180M Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | with hardener |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
Viscosity | 15000 - 32000 cP @Temperature 23.0 °C |
15000 - 32000 cP @Temperature 73.4 °F |
10 rpm |
Epoxy Technology EPO-TEK® B9021-6 Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Viscosity | 15000 - 23000 cP @Temperature 23.0 °C |
15000 - 23000 cP @Temperature 73.4 °F |
10 rpm |
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.Advantages & A.. |
|||
Viscosity | 15000 cP | 15000 cP | catalyzed with QM CAT RED 3 |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Viscosity | 15000 cP @Temperature 177 °C |
15000 cP @Temperature 350 °F |
Typical |
Bostik 2124 Flexible, Long Open Time EVA Glue Stick Bostik 2124 Flexible, Long Open Time EVA Glue StickFlexible. Long open time for most difficult substrates. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed (DV-III cp #52, 10 rpm) |
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive Information provided by Tra-Con Inc. |
|||
Viscosity | 15000 cP | 15000 cP | Part A, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1199 Black Unfilled Epoxy Adhesive Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Viscosity | 15000 - 20000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
15000 - 20000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK2.1° |
Gwent Electronic Materials D2090124D2 Green Solder mask Dielectric This product has been designed as a solder mask dielectric for use at high temperatures. It has been tested at 250°C and was proved to be stable for 12 weeks. Screen Printing Equipment: semi-automa.. |
|||
Viscosity | 15000 cP | 15000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Viscosity | 15000 cP | 15000 cP | Part A, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Viscosity | 15000 cP | 15000 cP | Part B, RVT, #6, 20 rpm; TM R050-12 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |