Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Taiwan PU Corporation PPG CPU-1090C Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Viscosity 15000 - 25000 cP

@Temperature 40.0 °C
15000 - 25000 cP

@Temperature 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
Tensile Strength at Break 19.12 - 28.93 MPa
2773 - 4196 psi
Elongation at Break 510 - 610 %
510 - 610 %
Tear Strength 83.4 - 123 kN/m
476 - 700 pli
Processing Properties Metric English Comments
Processing Temperature 85.0 °C
185 °F
Working Temperature, Prepolymer
Mold Temperature 100 °C
212 °F
Pot Life 10 min
10 min
Descriptive Properties Value Comments
MOCA Temperature 110°C
NCO Content Max 4.5%
Min 4.1%
PHR of MOCA 12.5%