| Category | Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset |
| Manufacturer | Tra-Con, Inc. |
| Trade Name | Tra-Duct |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Tra-Con Tra-Duct 2921 Silver-Filled Adhesive.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 3.67 g/cc | 3.67 g/cc | Mixed |
| Viscosity | 15000 cP <br>@Temperature 25.0 °C |
15000 cP <br>@Temperature 77.0 °F |
Mixed (DV-III cp #52, 10 rpm) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 70 | 70 | |
| Adhesive Bond Strength | 1.59 MPa | 230 psi | Lap shear, alum to alum, 1 hr @ 65°C |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | 6.75 °C | 44.2 °F | Ultimate Tg |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 1 hr @ 65°C |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 60.0 min <br>@Temperature 65.0 °C |
1.00 hour <br>@Temperature 149 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Silver | |
| Thixotropic Index | 1.6 | 1 rpm/10 rpm |