Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2000 - 4000 cP @Temperature 25.0 °C |
2000 - 4000 cP @Temperature 77.0 °F |
Uncured |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Viscosity | 3000 - 4000 cP @Temperature 25.0 °C |
3000 - 4000 cP @Temperature 77.0 °F |
Uncured |
Resin Technology Group UV-422 Flexible, UV Curing Sealant UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substr.. |
|||
Viscosity | 3000 - 4000 cP @Temperature 25.0 °C |
3000 - 4000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV640 UV-curable Adhesive PERMABOND UV640 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Viscosity | 50.0 - 4000 cP | 50.0 - 4000 cP | Average value: 578 cP Grade Count:9 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Viscosity | 3500 - 4000 cP | 3500 - 4000 cP | as supplied |
Industrial Nanotech Nansulateâ„¢ GP Translucent Insulation Coating Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.NANSULATEâ„¢ liquid applied insulation is a prem.. |
|||
Viscosity | 3500 - 4000 cP | 3500 - 4000 cP | as supplied |
Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATEâ„¢ liquid applied insulation is a premium industrial grade rust proofing protective .. |
|||
Viscosity | 3500 - 4000 cP | 3500 - 4000 cP | as supplied |
Industrial Nanotech Nansulateâ„¢ PT Translucent Insulation Coating Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.NANSULATEâ„¢.. |
|||
Viscosity | 1500 - 4000 cP @Temperature 40.0 °C |
1500 - 4000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PPG CPU-1060 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 3000 - 4000 cP | 3000 - 4000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A7020 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Viscosity | 3000 - 4000 cP @Time 7200 sec |
3000 - 4000 cP @Time 2.00 hour |
RP-0881 |
Solvay JAGUAR® C 14 S Surfactant Description: Substantive to hair and skin. Provides excellent wet combing and soft non-tacky feel to hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name : GUAR HYDROXYPROPYLTRIMONIUM CHLOR.. |
|||
Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U9081E Hardener Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 2000 - 4000 cP @Time 7200 sec |
2000 - 4000 cP @Time 2.00 hour |
RP-0942 |
Solvay JAGUAR® C 17 Surfactant Description: Highly substantive to hair and skin. Recommended for high conditioning shampoos and moisturizing body washes. Enhances deposition of actives such as silicone, anti-dandruff agents and m.. |
|||
Viscosity | 3000 - 4000 cP | 3000 - 4000 cP | |
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable .. |
|||
Viscosity | 1000 - 4000 cP | 1000 - 4000 cP | mixed compound |
Master Bond EP38CL Adhesive Features Toughness and Durability Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura.. |
|||
Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | Part A |
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no.. |
|||
Viscosity | 3000 - 4000 cP @Temperature 23.0 °C |
3000 - 4000 cP @Temperature 73.4 °F |
|
Master Bond EP21FL Flexibilized and Toughened Low Viscosity Epoxy Master Bond Polymer System EP21FL is a lower viscosity, two component, flexibilized epoxy resin system for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at r.. |
|||
Viscosity | 3000 - 4000 cP @Temperature 23.0 °C |
3000 - 4000 cP @Temperature 73.4 °F |
|
Master Bond EP30DP Abrasion Resistant Cryogenic Epoxy Urethane System Master Bond Polymer System EP30DP is a versatile, two component, epoxy-urethane elastomeric compound, featuring superior strength, toughness, and abrasion resistance for high performance bonding, se.. |
|||
Viscosity | 1000 - 4000 cP | 1000 - 4000 cP | Part B |
Master Bond EP30QF Quartz Filled, Two Component Epoxy System Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at.. |
|||
Viscosity | 2800 - 4000 cP | 2800 - 4000 cP | NOV QC 020 |
Lubrizol ESTANE® 5712F30 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 2000 - 4000 cP @Temperature 23.0 °C |
2000 - 4000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® EE149-6 Epoxy Material Description: A single component, silver-filled, B-stageable epoxy designed for semiconductor flip chip packaging or hybrid micro-electronic substrate attach or lid-sealing.Information Provi.. |
|||
Viscosity | 3000 - 4000 cP @Temperature 23.0 °C |
3000 - 4000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil.. |
|||
Viscosity | 2500 - 4000 cP @Temperature 23.0 °C |
2500 - 4000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |
|||
Viscosity | 2000 - 4000 cP @Temperature 23.0 °C |
2000 - 4000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H61 Unfilled Epoxy Adhesive Material Description: A single component, high Tg, electrically insulating epoxy adhesive for semiconductor, microelectronic, and opto-electronic packaging applications. It is a liquid version of E.. |
|||
Viscosity | 1000 - 4000 cP @Temperature 25.0 °C |
1000 - 4000 cP @Temperature 77.0 °F |
spindle n 3-10 RPM; MA143LFE |
C.O.I.M. FILCO® 368 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |