Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Industrial Nanotech Inc.
Trade Name Nansulate™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATE™ liquid applied insulation is a premium industrial grade rust proofing protective insulation coating containing Hydro-NM-Oxide. NANSULATE™, when fully cured, contains a high level of Hydro-NM-Oxide along with acrylic resin and performance additives. Nansulate has proven resistance to both existing mold growth and new mold growth. Nansulate can also be used for Lead Abatement—as a lead encapsulation coating. 20 year warranty.Uses: Pipes, Tanks, Trucks, Textile, Attics, Walls, Ships, Automotive, Containers, Residential, Commercial, IndustrialCorrosion protection and insulation are now combined into one, solving the costly problem of CUI (corrosion under insulation).Excellent adhesion to a wide variety of substrates.User-friendly with no special tools needed and easy to apply.Effective three-coat system, which can be easily over-coated if desired.Ability to see the substrate through the material allows for visual inspection of pipes, tank and equipment.Mold resistance without use of potentially harmful anti-fungal agentsEncapsulate Lead with a smooth, water-based, environmentally friendly coating.Information provided by Industrial Nanotech, Inc.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
as supplied
Solids Content 28 - 32 %
28 - 32 %
By Volume
30 - 34 %
30 - 34 %
By Weight
Viscosity 3500 - 4000 cP
3500 - 4000 cP
as supplied
Thickness 76.2 - 127 microns
3.00 - 5.00 mil
per coat; minimum three coats recommended
Thermal Properties Metric English Comments
Thermal Conductivity 0.0180 W/m-K
0.125 BTU-in/hr-ft²-°F
cured coating
Maximum Service Temperature, Air 204 °C
399 °F
cured coating
Processing Properties Metric English Comments
Processing Temperature 4.00 - 100 °C
39.2 - 212 °F
Application Temperature
Cure Time 60.0 - 120 min
1.00 - 2.00 hour
Hand Dry
1440 - 2880 min
24.0 - 48.0 hour
hard dry (return to service)
43200 - 86400 min
720 - 1440 hour
full cure
Descriptive Properties Value Comments
Color Translucent
Coverage per gallon 150 - 175 sq. ft. with three coats