Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7000 cP @Temperature 25.0 °C |
7000 cP @Temperature 77.0 °F |
|
Reltek BONDiT™ B-46CAT Adhesive and Sealant Key PropertiesExcellent adhesion to low surface energy plastics without primer or surface preparation.ApplicationsVery high flexibility, 500% elongation, emphasizing high tack for un-abraded substra.. |
|||
Viscosity | 7000 cP @Temperature 25.0 °C |
7000 cP @Temperature 77.0 °F |
|
Reltek BONDiT™ B-46TH Adhesive and Sealant Key PropertiesExcellent adhesion to low surface energy plastics without primer or surface preparation. ApplicationsVery high flexibility, 500% elongation, emphasizing high tack for un-abraded substr.. |
|||
Viscosity | 7000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
7000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Viscosity | 7000 cP | 7000 cP | Mixed; TM R050-12 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Viscosity | 7000 cP | 7000 cP | |
Ritelok RT20 High Temperature Retainer Anaerobic. High temp, retainer for auto/marine cylinder liners & heat exchange tubes. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Viscosity | 7000 cP @Temperature 175 °C |
7000 cP @Temperature 347 °F |
Shimadzu Viscosity, 1000 psi |
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Viscosity | 7000 - 20000 cP | 7000 - 20000 cP | |
Huntsman Araldite PZ 3901 Water-Based Adhesive/Coating Base Resin is GT 7071 (Type 1). Typical Solids Content 55%. Mean Particle Size |
|||
Viscosity | 7000 - 19000 cP | 7000 - 19000 cP | |
Huntsman MY 720 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: Tetra-functional liquid epoxy based on methylene dianiline. Excellent high temperature, chemical and radiation resista.. |
|||
Viscosity | 7000 - 10000 cP | 7000 - 10000 cP | |
Huntsman MY 9655 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: Narrow viscosity MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistant.. |
|||
Viscosity | 7000 - 11000 cP | 7000 - 11000 cP | |
Lord Adhesives 363 Two-Component, Fast Set, Modified Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 7000 cP @Temperature 25.0 °C |
7000 cP @Temperature 77.0 °F |
STM 1 |
Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easil.. |
|||
Viscosity | 7000 - 9000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
7000 - 9000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2030701P1 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. This is the most common ratio Material used for reference electrodes in medical diagnostics, environmental sensor and .. |
|||
Viscosity | 7000 - 11000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
7000 - 11000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C60903P5 Platinum Ink Platinum Ink designed for use as an internal electrode ink. For use with PVB Tapes. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-325 tpiSubstr.. |
|||
Viscosity | 7000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
7000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7355-9000 TPE Product Description: StarFlex P 7355-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Viscosity | 7000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
7000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7060-1000 TPE Product Description: StarMediflex P 7060-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Viscosity | 7000 - 13000 cP | 7000 - 13000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U101 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 7000 cP | 7000 cP | Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2 |
Formosa Plastics Formolon® 24A PVC PVC Homopolymer Dispersion Resin F-24A is a low molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compounds as well as other applica.. |
|||
Viscosity | 7000 cP | 7000 cP | |
Loctite® 277 High Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 7000 cP | 7000 cP | |
Esstech X-951-0080 BisGMA/Triethyleneglycol Dimethacrylate (80/20) To simplify the formulation processes, we provide bis GMA already diluted in a 80:20 ratio with TEGDMA. Bis-GMA and triethylene glycol dimethacrylate are commonly paired in dental formulations. Al.. |
|||
Viscosity | 7000 cP | 7000 cP | T |
Dymax 602 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Viscosity | 7000 cP | 7000 cP | |
Dymax 930 Coil Terminating, Tamper proofing and Structural Electronic Bonder High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 930 Coil Terminating, Tamper proofing and Structural Electronic BonderHigh strength, superior bonds to steel, alumin.. |
|||
Viscosity | 7000 cP | 7000 cP | |
3M Jet-Weld™ TE-015 Adhesive A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly.Extrudable. Very fast set time for bonding wood and selected plasticsInformation pro.. |
|||
Viscosity | 7000 cP | 7000 cP | |
ACC MM816 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 7000 - 16000 cP | 7000 - 16000 cP | Base |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Viscosity | 7000 cP | 7000 cP | Part A, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1026R Rubber Modified Epoxy Adhesive Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free .. |
|||
Viscosity | 7000 cP | 7000 cP | |
Resinlab® TL5077 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Viscosity | 7000 cP | 7000 cP | Part B (Polyol) |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Viscosity | 7000 cP | 7000 cP | Part B (Polyol) |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |
|||
Viscosity | <= 7000 cP | <= 7000 cP | |
Solvay MIRASHEEN® A-220 Surfactant Description: Liquid, cold pearl additive package that imparts opacity and pearlescence to formulated shampoos, liquid handsoaps, shower gels andrelated products. Requires no heat and readily blends .. |
|||
Viscosity | 7000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
7000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7330-1000 TPE Product Description: StarFlex P 7330-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |