STAR Thermoplastic Alloys & Rubbers StarMediflex P 7060-1000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarMediflex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarMediflex P 7060-1000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: StarMediflex P 7060-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:Soft TouchRubbery FeelExcellent ColorabilityProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Viscosity 7000 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
7000 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Time 10.0 sec
60

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 4.98 MPa

@Time 7200 sec
722 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 796 %

@Time 7200 sec
796 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00151 GPa

@Time 7200 sec
0.219 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 20.0 kN/m
114 pli
ASTM D624