Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300000 cP | 300000 cP | |
NextGen Adhesives P907-30 Optical Assembly Adhesive Description: NGAC P907-30 is a high viscosity, controlled flow encapsulant designed for microelectronics applications requiring low shrinkage and high reliability performance.Advantages and Applicat.. |
|||
Viscosity | 300000 cP @Shear Rate 190 1/s, Temperature 230 °C |
300000 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, .. |
|||
Viscosity | 300000 - 1.90e+6 cP @Shear Rate 50.0 - 50.0 1/s |
300000 - 1.90e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 495000 cP Grade Count:22 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Viscosity | 300000 cP | 300000 cP | Part B, Spindle TD, 2.5 rpm; Uncured |
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur.. |
|||
Viscosity | 300000 cP | 300000 cP | Part A, Spindle TD, 2.5 rpm; Uncured |
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Viscosity | 300000 cP | 300000 cP | Part B, Spindle TD, 2.5 rpm; Uncured |
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Viscosity | 300000 - 1.00e+6 cP | 300000 - 1.00e+6 cP | |
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 300000 - 400000 cP | 300000 - 400000 cP | Paste |
Lucas-Milhaupt Lucanex 616 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Viscosity | 300000 cP @Shear Rate 206 1/s, Temperature 200 °C |
300000 cP @Shear Rate 206 1/s, Temperature 392 °F |
ASTM D3835 |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Viscosity | 300000 cP @Temperature 25.0 °C |
300000 cP @Temperature 77.0 °F |
Mixed (cp #52, 1 rpm) |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Viscosity | 300000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
300000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 1124 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Viscosity | 300000 cP | 300000 cP | |
Loctite® PST® 565 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 300000 - 500000 cP | 300000 - 500000 cP | Dynamic |
Dow Corning 9041 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and w.. |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F130-E5 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 300000 cP @Temperature 190 °C |
300000 cP @Temperature 374 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1377E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 300000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® XP36-E1 PA6 Film Extrusion, Medium Viscosity, Nucleated, Lubricated |
|||
Viscosity | 300000 - 800000 cP | 300000 - 800000 cP | Part B |
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat.. |
|||
Viscosity | 300000 cP | 300000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |
|||
Viscosity | 300000 cP @Temperature 400 °C |
300000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |