Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 15000 - 30000 cP @Temperature 25.0 °C |
15000 - 30000 cP @Temperature 77.0 °F |
Uncured |
Permabond ES562 Epoxy Resin PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t.. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed |
Resin Technology Group KONA 871 Low Cost Epoxy Resin Mix ratio 100 to 25 by weight.Kona 871 is a low cost epoxy resin system developed for production casting, potting, encapsulating and coating applications where easy handling, good flowability and lo.. |
|||
Viscosity | 15000 - 30000 cP @Temperature 25.0 °C |
15000 - 30000 cP @Temperature 77.0 °F |
|
Lucite International Colacryl ® TS1631 Acrylic Solution Resin Acrylic copolymer with reactive groupsA highly flexible resin with good handle. It exhibits good adhesion, resistance to ageing and light stability.Suggested Use: Coating and lamination of nylon and.. |
|||
Viscosity | 15000 cP | 15000 cP | Before Curing |
Silikony Polskie Gumosil K Silicone Rubber Flexible with good tearing resistance |
|||
Viscosity | 15000 - 60000 cP | 15000 - 60000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U0251M Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | <= 15000 cP | <= 15000 cP | #3 SP @ 12 rpm; RP-0596 |
Solvay MIRASHEEN® CP-820 Surfactant Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related produ.. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 15 LV Clear Variable Hardness Low Viscosity Catalyst Emerson & Cuming 15 LV Clear Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener .. |
|||
Viscosity | 15000 cP | 15000 cP | Part B |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Viscosity | 15000 - 30000 cP | 15000 - 30000 cP | Part A |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 3180M Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Viscosity | 15000 cP | 15000 cP | dynamic, mixing |
Dow Corning HS III BASE & 10:1 COLORED CATALYST High strength lower durometer silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS III Base with HS III 10:1 Colored Catalyst is recommended.. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | with hardener |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
Viscosity | 15000 - 18000 cP @Temperature 23.0 °C |
15000 - 18000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2101 is a two component, thixotropic, electrically conductive adhesive. It may be used for circuit assembly and semiconductor applications. Advantages & Application .. |
|||
Viscosity | 15000 cP | 15000 cP | Mixed |
Armstrong A-2/H20 Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Viscosity | 15000 cP | 15000 cP | catalyzed with QM CAT PURPLE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Viscosity | 15000 cP | 15000 cP | |
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | ASTM D562 |
Asia Technology Pioneers CAN 102 Acrylic Hi-Compound Resin Description: ACN 102 is hi-tech compounded Acrylic Resin. This hi-composite is produced by Nano-Technology and used widely in paint and Coating industryAdvantages:High abrasion and corrosion resista.. |
|||
Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
Mixed (DV-III cp #52, 10 rpm) |
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive Information provided by Tra-Con Inc. |
|||
Viscosity | 15000 cP | 15000 cP | Base |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 15000 - 55000 cP | 15000 - 55000 cP | |
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Viscosity | 15000 cP | 15000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |