Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Melt Index of Compound | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Melt Index of Compound | 33 g/10 min @Load 10.0 kg, Temperature 210 °C |
33 g/10 min @Load 22.0 lb, Temperature 410 °F |
|
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |
|||
Melt Index of Compound | 33 g/10 min @Load 5.00 kg, Temperature 280 °C |
33 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V9561 PET Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Melt Index of Compound | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Melt Index of Compound | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Melt Index of Compound | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Melt Index of Compound | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Melt Index of Compound | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Melt Index of Compound | 33 g/10 min | 33 g/10 min | ASTM D1238 |
Cheng Yu Plastic 3276 TPE Rubber |
|||
Melt Index of Compound | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Melt Index of Compound | 33 g/10 min @Load 5.00 kg, Temperature 280 °C |
33 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |