Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs XX0 ABS, Extrusion Grade Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC GF3020 PB7 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East) LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East) LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYform POM C M20 AS4 Polyoxymethylene, Antistatic Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 155-1339 LMDPE Rotational Molding Resin Description: ICORENE 155-1339 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Melt Index of Compound | 3.0 g/10 min @Temperature 230 °C |
3.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Mitsui ADMER® QB510A PP Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 3.0 g/10 min @Temperature 230 °C |
3.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Mitsui ADMER® QF500A PP Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 3.0 g/10 min | 3.0 g/10 min | |
Lushan AR-10 Nylon Toughener/PA Impact Modifier Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener.. |
|||
Melt Index of Compound | 3.0 g/10 min @Temperature 190 °C |
3.0 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® NF498A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East) PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)... |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
3.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 4522 Halogen Free PVC High flame retardancy |
|||
Melt Index of Compound | 3.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
3.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
|
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6303Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Melt Index of Compound | 3.0 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-03 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melt Index of Compound | 3.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Melt Index of Compound | 3.0 g/10 min | 3.0 g/10 min | |
Lushan OR-1 Halogen-Free Flame-Retardant Compatibilizer Halogen-free flame retardant compatibilizer Lushan series for cables and wires are developed by several doctors and maters from Lushan’s R&D Center, and combined ten years’ modified polyolefin gra.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HI835M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |