Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 230 °C |
22 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs S00 ABS, High Flow Information provided by Polykemi AB |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 230 °C |
22 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs S00 AS UV ABS, High Flow, UV-Stabilized, Antistatic Information provided by Polykemi AB |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 230 °C |
22 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs S20 ABS Information provided by Polykemi AB |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Melt Index of Compound | >= 22 g/10 min @Load 2.16 kg, Temperature 260 °C |
>= 22 g/10 min @Load 4.76 lb, Temperature 500 °F |
cm³/10min; ISO 1133 |
PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Melt Index of Compound | 22 g/10 min | 22 g/10 min | ASTM D1238 |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Melt Index of Compound | 22 g/10 min | 22 g/10 min | ASTM D1238 |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 300 °C |
22 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 300 °C |
22 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 300 °C |
22 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 250 °C |
22 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 265 °C |
22 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P55B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Melt Index of Compound | 22 - 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 28-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melt Index of Compound | 22 - 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 224 °C |
22 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |