Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Melt Index of Compound | 1.0 g/10 min @Temperature 190 °C |
1.0 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® NF458A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 1.0 - 3.0 g/10 min | 1.0 - 3.0 g/10 min | |
Sibur ABS 1106 Extrusion Grade ABS Plastic With high deformation properties and sanitary-hygienic properties for production of sheets with following pneumatic and vacuum forming of internal parts of refrigerators, as well as for compounding .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | |
Sibur MPP 15-06V Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | |
Sibur MPP 21015-E10 Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8107 Polyolefin Elastomer Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8842 Polyolefin Elastomer Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle si.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1137 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1137 NT 7 is an ethylene copolymer intended for use in molding and extrusion applications where high flexibility is desired. It is especially useful for flexible hose and tube appli.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber Description: This crystalline ethylene-propylene-diene terpolymer (EPDM) has a low viscosity for excellent flow characteristics and hot green strength. It has been designed for property modification.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Arkema Group OREVAC® 18334 Grafted Maleic Anhydride Polyethylene OREVAC 18334 is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier bottle. OREVAC 18334 is mainly used in multi-layer bottle and tank to have good adhesio.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Cond. E; ISO 1133 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Cond. E; ISO 1133 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8540 Polyolefin Elastomer Description: Engage® 8540 polyolefin elastomer is an ethyleneoctene copolymer that is well suited to foamed applications and offers excellent performance for profile extrusion of tubing and hoses. .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |