Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 6.35 mm |
0.012 - 0.014 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.17 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.17 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.011 - 0.014 cm/cm @Thickness 3.17 mm |
0.011 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.00 mm |
0.012 - 0.014 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 341 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.014 cm/cm @Thickness 3.00 mm |
0.012 - 0.014 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm |
0.0090 - 0.014 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.014 cm/cm @Thickness 1.60 mm |
0.0080 - 0.014 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |