Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0050 - 0.0060 cm/cm @Thickness 3.17 mm |
0.0050 - 0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 4115-104D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0060 cm/cm @Thickness 6.35 mm |
0.0050 - 0.0060 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/15/UV/HS Polypropylene Homopolymer, 15% Glass Reinforced, Heat Stabilized, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 3.00 mm |
0.0030 - 0.0060 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 3.00 mm |
0.0030 - 0.0060 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm @Thickness 1.60 mm |
0.0030 - 0.0060 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |