Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.013 cm/cm @Thickness 3.17 mm |
0.013 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.013 - 0.017 cm/cm @Thickness 3.17 mm |
0.013 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.013 - 0.017 cm/cm @Thickness 3.17 mm |
0.013 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm @Thickness 6.35 mm |
0.013 - 0.016 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.013 cm/cm @Thickness 6.35 mm |
0.013 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.013 cm/cm @Thickness 3.20 mm |
0.013 in/in @Thickness 0.126 in |
Transverse |
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide.. |