Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | LATI |
LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic
(discon Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Aardvark Polymers AARTEL® 800 Rotational Molding Resin Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of st.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12 LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing 20% Aramid. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.021 cm/cm @Time 86400 sec |
0.020 - 0.021 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.050 cm/cm @Time 86400 sec |
0.020 - 0.050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 901 MS POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 902 FA POM Copolymer unreinforced, reduced formaldehyde emission, UV-stabilized POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Diameter 2.00 mm |
0.020 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Diameter 2.00 mm |
0.020 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Diameter 2.00 mm |
0.020 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
DSM Arnite® T06 202 /A PBT Medium Viscosity, Injection Molding |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
DSM Stanyl® TE300 PA46 Heat Stabilized |