Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0150 cm/cm | 0.00500 - 0.0150 in/in | Average value: 0.00940 cm/cm Grade Count:10 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00700 cm/cm | 0.00500 - 0.00700 in/in | Average value: 0.00600 cm/cm Grade Count:8 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00600 cm/cm | 0.00500 - 0.00600 in/in | Average value: 0.00550 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00950 cm/cm | 0.00500 - 0.00950 in/in | Average value: 0.00752 cm/cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0240 cm/cm | 0.00500 - 0.0240 in/in | Average value: 0.0171 cm/cm Grade Count:8 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0110 cm/cm | 0.00500 - 0.0110 in/in | Average value: 0.00792 cm/cm Grade Count:13 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.100 cm/cm | 0.00500 - 0.100 in/in | Average value: 0.0118 cm/cm Grade Count:62 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0105 cm/cm | 0.00500 - 0.0105 in/in | Average value: 0.00819 cm/cm Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0100 cm/cm | 0.00500 - 0.0100 in/in | Average value: 0.00768 cm/cm Grade Count:11 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0165 cm/cm | 0.00500 - 0.0165 in/in | Average value: 0.00972 cm/cm Grade Count:9 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00900 cm/cm | 0.00500 - 0.00900 in/in | Average value: 0.00770 cm/cm Grade Count:5 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0170 cm/cm | 0.00500 - 0.0170 in/in | Average value: 0.0113 cm/cm Grade Count:11 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |