Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0041 cm/cm | 0.0041 in/in | |
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage, Transverse | 0.0041 cm/cm @Time 86400 sec |
0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Linear Mold Shrinkage, Transverse | 0.0041 cm/cm | 0.0041 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Linear Mold Shrinkage, Transverse | 0.0041 cm/cm @Time 86400 sec |
0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00CE is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0041 cm/cm @Time 86400 sec |
0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Verton UV00ASXS PPA (Europe-Africa-Middle East) LNP* VERTON* UV00ASXS is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |