Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0220 cm/cm | 0.00400 - 0.0220 in/in | Average value: 0.0130 cm/cm Grade Count:44 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0140 cm/cm | 0.00400 - 0.0140 in/in | Average value: 0.00876 cm/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0190 cm/cm | 0.00400 - 0.0190 in/in | Average value: 0.0104 cm/cm Grade Count:14 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00654 cm/cm Grade Count:13 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0100 cm/cm | 0.00400 - 0.0100 in/in | Average value: 0.00650 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00750 cm/cm | 0.00400 - 0.00750 in/in | Average value: 0.00593 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0189 cm/cm | 0.00400 - 0.0189 in/in | Average value: 0.00895 cm/cm Grade Count:28 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0180 cm/cm | 0.00400 - 0.0180 in/in | Average value: 0.0120 cm/cm Grade Count:9 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00677 cm/cm Grade Count:95 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00580 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00550 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0110 cm/cm | 0.00400 - 0.0110 in/in | Average value: 0.00788 cm/cm Grade Count:10 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0206 cm/cm | 0.00400 - 0.0206 in/in | Average value: 0.0109 cm/cm Grade Count:17 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |