Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00467 cm/cm Grade Count:3 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00592 cm/cm Grade Count:24 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00333 cm/cm Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00640 cm/cm | 0.00200 - 0.00640 in/in | Average value: 0.00570 cm/cm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00400 cm/cm | 0.00200 - 0.00400 in/in | Average value: 0.00283 cm/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00429 cm/cm Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00750 cm/cm | 0.00200 - 0.00750 in/in | Average value: 0.00442 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00557 cm/cm Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00545 cm/cm Grade Count:34 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00545 cm/cm Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00740 cm/cm Grade Count:20 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.100 cm/cm | 0.00200 - 0.100 in/in | Average value: 0.0150 cm/cm Grade Count:30 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0122 cm/cm | 0.00200 - 0.0122 in/in | Average value: 0.00844 cm/cm Grade Count:13 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0180 cm/cm | 0.00200 - 0.0180 in/in | Average value: 0.0113 cm/cm Grade Count:15 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00544 cm/cm Grade Count:11 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0400 cm/cm | 0.00200 - 0.0400 in/in | Average value: 0.0111 cm/cm Grade Count:94 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00600 cm/cm Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0253 cm/cm | 0.00200 - 0.0253 in/in | Average value: 0.0156 cm/cm Grade Count:62 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0130 cm/cm | 0.00200 - 0.0130 in/in | Average value: 0.00812 cm/cm Grade Count:47 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0400 cm/cm | 0.00200 - 0.0400 in/in | Average value: 0.0143 cm/cm Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |