Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0135 cm/cm | 0.00250 - 0.0135 in/in | Average value: 0.00644 cm/cm Grade Count:37 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 - 0.0135 cm/cm | 0.0095 - 0.0135 in/in | |
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;.. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 - 0.0135 cm/cm | 0.0095 - 0.0135 in/in | |
LATI Latilub 62-06GR PA6, Graphite Reinforced Self-lubricating product based on Polyamide 6 (PA6). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.0135 cm/cm | 0.010 - 0.0135 in/in | |
LATI Latilub 62-10T PA6 Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latimass 66-04 D009 PBT Specific density compound based on Polybutylene Terephthalate (PBT). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latistat 62-06 K/10 PA6, 10% Carbon Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Linear Mold Shrinkage, Transverse | 0.0095 - 0.0135 cm/cm | 0.0095 - 0.0135 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1811-BK1 15% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latimass 52/11-04 D008 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.0135 cm/cm | 0.010 - 0.0135 in/in | |
LATI Latiohm 66-10 H2 CNT G/35 PA66, 35% Glass Fiber Reinforced, Heat Stabilized Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0135 cm/cm | 0.0115 - 0.0135 in/in | |
LATI Latilub 95-15T PSU, PTFE Filled Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |