Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.20 mm
0.0045 - 0.0065 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 3412HF PC
20% glass reinforced, high flow PC. UL rated V-1 at 0.059"",
Linear Mold Shrinkage, Transverse 0.0050 - 0.0065 cm/cm
0.0050 - 0.0065 in/in
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Linear Mold Shrinkage, Transverse 0.0040 - 0.0065 cm/cm
0.0040 - 0.0065 in/in
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
0.0045 - 0.0065 in/in
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
0.0045 - 0.0065 in/in
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Linear Mold Shrinkage, Transverse 0.0040 - 0.0065 cm/cm
0.0040 - 0.0065 in/in
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi..
Linear Mold Shrinkage, Transverse 0.0040 - 0.0065 cm/cm
0.0040 - 0.0065 in/in
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Linear Mold Shrinkage, Transverse 0.0040 - 0.0065 cm/cm
0.0040 - 0.0065 in/in
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
0.0045 - 0.0065 in/in
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
0.0045 - 0.0065 in/in
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
0.0045 - 0.0065 in/in
LATI Lastilac AR-V0E ABS, Flame Retardant
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0065 cm/cm
0.0050 - 0.0065 in/in
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced
High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
0.0045 - 0.0065 in/in
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria ..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.20 mm
0.0045 - 0.0065 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.20 mm
0.0045 - 0.0065 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Linear Mold Shrinkage, Transverse 0.0053 - 0.0065 cm/cm

@Time 86400 sec
0.0053 - 0.0065 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS
LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0060 - 0.0065 cm/cm

@Time 86400 sec
0.0060 - 0.0065 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DX11354 PC (Asia Pacific)
This is a PC compound with good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications.
Linear Mold Shrinkage, Transverse 0.0053 - 0.0065 cm/cm

@Time 86400 sec
0.0053 - 0.0065 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific)
LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.00 mm
0.0045 - 0.0065 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® FR3005 HG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.00 mm
0.0045 - 0.0065 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® FR3009 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm

@Thickness 3.20 mm
0.0045 - 0.0065 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific)
20% glass reinforced, high flow PC. UL rated V-1 at 0.059"",
Linear Mold Shrinkage, Transverse 0.0050 - 0.0065 cm/cm
0.0050 - 0.0065 in/in
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced
High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0065 cm/cm
0.0050 - 0.0065 in/in
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant
High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid..
Linear Mold Shrinkage, Transverse 0.0025 - 0.0065 cm/cm
0.0025 - 0.0065 in/in
LATI Latigea B01 I6 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...