Polymer Property : Linear Mold Shrinkage, Transverse = 0.00100 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cm
0.00100 - 0.0190 in/in
Average value: 0.00861 cm/cm Grade Count:23
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.0107 cm/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0160 cm/cm
0.00100 - 0.0160 in/in
Average value: 0.00953 cm/cm Grade Count:32
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.0103 cm/cm Grade Count:80
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0210 cm/cm
0.00100 - 0.0210 in/in
Average value: 0.00968 cm/cm Grade Count:124
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00566 cm/cm Grade Count:33
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00750 cm/cm
0.00100 - 0.00750 in/in
Average value: 0.00486 cm/cm Grade Count:30
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00546 cm/cm Grade Count:35
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cm
0.00100 - 0.00500 in/in
Average value: 0.00425 cm/cm Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0140 cm/cm
0.00100 - 0.0140 in/in
Average value: 0.00752 cm/cm Grade Count:33
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0158 cm/cm
0.00100 - 0.0158 in/in
Average value: 0.00839 cm/cm Grade Count:52
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.0127 cm/cm Grade Count:19
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00580 cm/cm Grade Count:26
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00708 cm/cm Grade Count:6
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cm
0.00100 - 0.00500 in/in
Average value: 0.00300 cm/cm Grade Count:3
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00425 cm/cm Grade Count:19
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.00300 cm/cm
0.00100 - 0.00300 in/in
Average value: 0.00250 cm/cm Grade Count:4
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cm
0.00100 - 0.0190 in/in
Average value: 0.0127 cm/cm Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0120 cm/cm
0.00100 - 0.0120 in/in
Average value: 0.00697 cm/cm Grade Count:37
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm

@Temperature 150 - 150 °C
0.00100 - 0.0100 in/in

@Temperature 302 - 302 °F
Average value: 0.00500 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm

@Time 900 - 900 sec
0.00100 - 0.0100 in/in

@Time 0.250 - 0.250 hour
Average value: 0.00500 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0120 cm/cm
0.00100 - 0.0120 in/in
Average value: 0.00879 cm/cm Grade Count:13
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..