Material Notes:
Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 81 - 87
81 - 87
delayed; ASTM D-2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D-638
Elongation at Yield 279.5 %
279.5 %
Air Aging: 7 days @ 136°C; 30 mil slabs; UL 1581
279.8 %
279.8 %
Oil Aging: 7 days @ 60°C; IRM 902 oil; 30 mil slabs; UL 1581
340 %
340 %
ASTM D-638
100% Modulus 0.009480 GPa
1.375 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F