Michelman® Licomer® M 63 Styrene-Acrylate copolymer dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Licomer®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Licomer® M 63 Styrene-Acrylate copolymer dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 63 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. This product provides excellent gloss, good traffic resistance on large surfaces, easy buffability with 'ultra-high-speed' machines, good dirt repellence and low presence of black heel marks, excellent removal with ammonium cleaning agents, and excellent mechanical properties.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.06 - 1.08 g/cc
1.06 - 1.08 g/cc
Volatiles 59 - 61 %
59 - 61 %
pH 8.0 - 9.5
8.0 - 9.5
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Milky white liquid
Emulsifier Charge Anionic/Nonionic
Solids Type Styrene Acrylate Copolymer