Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.35 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D792
S&E Specialty Polymers GA-1046CTLF PVC
Application: Lead free 105° C tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SRPVC, MIL-I-16878.Information provided by S&E Specialty Polymers
Specific Gravity 1.33 - 1.35 g/cc
1.33 - 1.35 g/cc
PEPL-10-W-21
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Specific Gravity 1.25 - 1.35 g/cc

@Thickness 1.57 mm
1.25 - 1.35 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
NBR NM-IEC 60811-1-3
Karina SDB 40/1-HSF Ivory PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.30 - 1.35 g/cc

@Thickness 1.57 mm
1.30 - 1.35 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP600 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062"..
Specific Gravity 1.30 - 1.35 g/cc

@Thickness 1.57 mm
1.30 - 1.35 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP602 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne..
Specific Gravity 1.30 - 1.35 g/cc

@Thickness 1.57 mm
1.30 - 1.35 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP605 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is normally used in the printed circuit board industry as a backup for the drilling operatio..
Specific Gravity 1.30 - 1.35 g/cc

@Thickness 1.57 mm
1.30 - 1.35 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP613 Paper Base Laminate
Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels..
Specific Gravity 1.30 - 1.35 g/cc

@Thickness 1.57 mm
1.30 - 1.35 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina 36/19-FC-LMP (SDB) Brown Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina 752-12/6-Y-BZ Ruby Red PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina 800-DA-10/1-A-AT-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina 951-35/4-IS-LMP Ivory PVC Compound
Heavy metal free PVC compound with high electrical insulation resistance. Recommended for insulation of CI and CCI cables.Information provided by Karina Indústria e Comércio de Plásticos Lt..
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina E 105908-35/1-C-IS-LMP Ivory PVC Compound
PVC compound recommended for extrusion of wires TW and THW.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina E 800D10/7-A-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina E 802-IS-SD Clear PVC Compound
PVC compound developed for films (non-toxic).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina 800D10/7-A-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Karina E 700-08/166-B Beige PVC Compound
For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 53061A Moldings & Extrusions Flexible PVC
General purpose injection molding and extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 8644 Moldings & Extrusions Flexible PVC
General purpose extrusion compound. Forms a good bond with rigid PVC in co-extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 15640 Wire & Cable Flexible PVC
Semi-rigid UL style #1061.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 50897 Moldings & Extrusions Flexible PVC
Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 8802 Moldings & Extrusions Flexible PVC
General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 19810 Wire & Cable Flexible PVC
Primary insulation also recommended for 105°C molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 19920 Wire & Cable Flexible PVC
Non-lead stabilized 105°C insulation compound recommended for THHN-THWN circuit sizes. Well suited for 105°C; 1/64 wall in all AWG sizes. CSA approved for FT1 TWN75, TEW and AWM IA constructions..
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 8741 Moldings & Extrusions Flexible PVC
A low gravity general purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axi..
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 8863 Moldings & Extrusions Flexible PVC
A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles and tubings. Meets the requirements for LP Gas hose per UL21.Information provided by Georgia ..
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D792
Compuestos Dominicanos Polycom BD-220699 PVC Compound
The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar..
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 15900 Wire & Cable Flexible PVC
Non-lead stabilized insulation compound recommended for TW and 80C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Axiall 18660 Moldings & Extrusions Flexible PVC
Flame retardant extrusion and molding compound recommended for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Copyright © lookpolymers.com All Rights Reserved