Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers G-04-036ESD PVC Application: High Performance, PVC based compound with antistatic properties. G-04-036ESD is suitable for Gamma radiation sterilization.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers G-3085E PVC Application: General purpose PVC material with good low temperature properties designed for T-Molding extrusion applicationsInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers GA-1050-OR3-LF PVC Application: Lead free, 105° C PVC insulating compound designed for SJEOO applications. Complies with RoHS requirements.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers GR-1409 PVC Application: High flow, high impact rigid PVC based compound. It is suitable for injection molding of the large parts.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ISO 1183 |
PTS PBT-1100A PBT Resin Information provided by PTS LLC. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina KAPU 8035/1-Y Ivory PVC Compound Foamed PVC compound to be used like an alternative to PU for injection of extra-light shoes soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 552-48/1-DT-IE Compound PVC Black PVC Compound for shoe industry with fruit scentInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 552-48/1-DT-IE Compound PVC Black PVC compound for shoe industry with fruit scent.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D 792 |
Karina 600-DA-48/1-C-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina 651-48/1-BY-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 651D10/1-C-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 900-35/1-AYR-AC-LF Ivory PVC Compound Flame retardant and heavy metal free PVC compound, recommended for insulation of automotive electrical cables for working at the temperature range of -40°C to 105°C.Information provided by Kar.. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 901D10/146-B-AT White PVC Compound Non toxic PVC compound recommended for injection of parts for general applications.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 40/272-FC-LMP Green Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 42/234-FC-LMP MB Concentration de Pigment Red for PVC Pigment Concentrate Recommended for Extrusion General PVC. Minimum usage 2%. Organic and Inorganic.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E 45/28-GEN Gold MB (SP31471) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina 40/272-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E 858-10/16-ERYA PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 68141 Wire & Cable Flexible PVC 90°C rated, non-lead stabilized compound designed for use as an SE and USE jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 16782 Wire & Cable Flexible PVC Non-lead stabilized, 90C jacketing compound with excellent low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ISO 1183 |
BLUESTAR PBT 1100A Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 21572 Coax & Telecom Flexible PVC Semi-rigid non-lead stabilized insulation compound designed for data communication riser cable applications. Maximum 60°C service temperature rating.Information provided by Georgia GulfGeorgia Gul.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 22561 Coax & Telecom Flexible PVC Non-lead stabilized, semi-rigid insulation compound for minimum transmission interference in communication applications. Suitable for use as a riser insulation.Information provided by Georgia GulfG.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 50896 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 12870 Wire & Cable Flexible PVC 70°C oil, 80°C dry rated liquid tight conduit jacket meeting the requirements of UL 360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 19730 Wire & Cable Flexible PVC Electrical grade 105°C rated vinyl elastomer compound suitable for SEO and SJEO insulation and jacket applications per UL 62.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 19732 Wire & Cable Flexible PVC Non-lead stabilized, electrical grade 105°C rated non-lead vinyl elastomer compound suitable for SEO and SJEO insulation and jacket applications per UL 62.Information provided by Georgia GulfGeorgi.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D792 |
BLUESTAR PBT 1090 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 4590 Flexible PVC 10 mil automotive thin wall insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 4470 Flexible PVC High speed ultrathinwall automotive harness wire per SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |