Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E 45/28-GEN Gold MB (SP31471) for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 45/28-GEN Gold MB (SP31471) for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D 792
ASTM Color 13.45 - 16.45
13.45 - 16.45
Color A, ME 12
40.38 - 43.38
40.38 - 43.38
Color B, ME 12
59.31 - 62.31
59.31 - 62.31
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 48 - 52

@Time 15.0 sec
48 - 52

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Extrusion