| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant |
| Manufacturer | Polymer Technology & Services, LLC (PTS) |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PTS PBT-1100A PBT Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ISO 1183 |
| Moisture Absorption at Equilibrium | <= 0.3 % | <= 0.3 % | ISO 15512 |
| Viscosity Measurement | 1.03 - 1.07 | 1.03 - 1.07 | cm<sup>3<sp>/g; ISO 1628/5 |
| Ash | <= 0.035 % | <= 0.035 % | ISO 3451/1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 222 - 226 °C | 432 - 439 °F | ISO 11357 |
| 222 - 226 °C | 432 - 439 °F | ISO 11357 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | <= 0.30 % | <= 0.30 % | ISO 15512 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Carloxyl End Groups | < 30 mol/t | Q/NHS 501 |
| Color B | < 6.0 | Hunter Lab |