Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Alumex™ Kaolin Alumex is a Hydrated Aluminum Silicate used as a low surface area “soft†filler for Elastomeric systems.Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Kaolexâ„¢ FG Kaolin Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Kaolexâ„¢ SC Kaolin Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Minsparâ„¢ 10 Ground Feldspar Minsparâ„¢ 10 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 10 is easily dispersed to a high Hegman grind to produce coatings finish.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Minsparâ„¢ 7 Ground Feldspar Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-d Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 70°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 35B Kaolin Clay - Waterwashed Coarsest kaolin with the lowest oil absorption, for excellent extension without frosting in water-based coatings. Spray dried bead form.Industry: Paint & Coatings, Adhesives & SealantsUses: Architec.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Nulok® 390 Kaolin Clay - Surface Treated High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® 70 Kaolin Clay - Calcined Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® DLX Kaolin Clay - Delaminated Polyfil DLX is a large particle size, very high aspect ratio, delaminated clay that reduces gas and vapor permeability. It is a type of water washed clay which is processed to have a high aspect rat.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline Dedusted Flake Series DF-2750 Aluminum Flake DF-2750 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with an uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dus.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline Dedusted Flake Series DF-3500 Aluminum Flake DF-3500 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with an uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dus.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 3101X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 4852X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 6802X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | Cured |
Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy TRA-DUCT 925M01 is a low ion snap cure silver-filled epoxy. TRA-DUCT 925M01 develops strong, durable, void free electrically and thermally conducting bonds. The product can be screen printed, stenci.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | ASTM D792 |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | cured |
Atom Adhesives AA-DUCT 906 Epoxy Adhesive AA-DUCT 906 represents the newest technology since the introduction of electrically conductive silver compounds. This unique formulation is based on a silver coated ceramic that results in lower mat.. |