Material Notes:
SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance properties in the final coating.Applications: Powder Coatings
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Volatiles 1.0 %
1.0 %
Particle Size 36 µm
36 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh