Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KaMin Nulok® 390 Kaolin Clay - Surface Treated

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Nulok® 390 Kaolin Clay - Surface Treated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, Thermoset, Thermoplastic, EPDM, Wire & CableInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 91 %
91 %
Reflectance (TAPPI)
Moisture Absorption at Equilibrium <= 1 %
<= 1 %
As Produced
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
0.400 µm
0.400 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.05% Retained
pH 8.5
8.5
100 g/250 ml H2O Slurry
Specific Surface Area 22.0 m²/g
22.0 m²/g
BET
Descriptive Properties Value Comments
CAS Number Proprietary
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved