Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.91 g/cc | 1.91 g/cc | ASTM D792 |
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet) Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | TM R050-16 |
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | TM R050-16 |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Specific Gravity | 1.91 - 2.01 g/cc | 1.91 - 2.01 g/cc | NBR NM-IEC 60811-1-3 |
Karina White Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® 760-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® 793-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® 883-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® Premier 860-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® Premier 890-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® Premier 910-20-C Aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited of use in liquid colorant applic.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Sparkle Silvex® Premier 838-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Tufflake® 2222-AR Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | |
Silberline Tufflake® 2722 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Specific Gravity | 1.91 g/cc | 1.91 g/cc | at 25°C |
Daikin DAI-EL G-575 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 70% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low permeability to gasoline and a.. |
|||
Specific Gravity | 1.91 - 1.97 g/cc | 1.91 - 1.97 g/cc | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Specific Gravity | 1.91 - 1.97 g/cc | 1.91 - 1.97 g/cc | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Specific Gravity | 1.91 - 1.93 g/cc | 1.91 - 1.93 g/cc | |
PolyChem Alloy PolyGard 7507N PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph.. |