Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.80 - 1.95 g/cc | 1.80 - 1.95 g/cc | |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Specific Gravity | 1.80 - 1.95 g/cc | 1.80 - 1.95 g/cc | |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | |
Parker Chomerics CHO-SHIELD® 4916 Conductive Coating Conductive CoatingInformation provided by Chomerics |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Parker Chomerics CHO-SHIELD® 576 Platable Silver Epoxy Coating Description: CHO-SHIELD® 576 coating is a two component, silver filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric plastic substrate. This coating .. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ISO 1183 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Premix Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontin Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Haysite H900 Polyester, Glass Reinforced H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,.. |
|||
Specific Gravity | 1.80 - 1.84 g/cc | 1.80 - 1.84 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS2603 Fluoroelastomer Copolymer Gum Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc.. |
|||
Specific Gravity | 1.80 - 1.84 g/cc | 1.80 - 1.84 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS2604 Fluoroelastomer Copolymer Gum Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ 2299X Ultra High Viscosity Fluoroelastomer 3M™ Dyneon™ FC 2299X is an ultra high viscosity fluoroelastomers designed for use in applications such as o-rings, gaskets and seals requiring higher strength than achievable with lower viscosity .. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2174 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2174 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2179 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2179 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FE 5643Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5643Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FG 5690Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FG 5690Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | ASTM D792 |
Cheng Yu Plastic E2345 Flame Retardant PET, 45% Glass Fiber |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
Bulk Molding Compounds BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled Description: BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compress.. |
|||
Specific Gravity | 1.80 g/cc | 1.80 g/cc | |
3M Dyneon™ FC 2211 Fluoroelastomer Dyneon FC 2211 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The "dry" ingre.. |
|||
Specific Gravity | 1.80 - 2.00 g/cc | 1.80 - 2.00 g/cc | ISO 1183 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |