Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.66 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Gromax PBT 4130-201D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
LG Chemical Lupox® GP2306FY PBT+GF30%
Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific)
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline EternaBrite® Premier 251-PA
EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline EternaBrite® Premier 255-PA
EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline Sparkle Silvex® 963-30-C
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Samsung Cheil Industries Infino® XP-2140 PPS
Information provided by Samsung Cheil Industries.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp WB008 PBT
LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Specific Gravity 1.66 - 1.70 g/cc
1.66 - 1.70 g/cc
ASTM D-792
Axiall H 3138A Plenum Flexible PVC
Plenum-grade Category 3 jacket. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
E-Polymers SEPAZ® V330FR 30% Glass Fiber Reinforced Flame Retardant PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Samsung Cheil Industries Infino® XP-2140 PPS
Information provided by Samsung Cheil Industries.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Samsung Cheil Industries Infino® XP-2140C PPS
Information provided by Samsung Cheil Industries.