Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | Method A; ASTM D792 |
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Specific Gravity | 1.64 - 1.70 g/cc | 1.64 - 1.70 g/cc | ASTM D 792 |
Karina 18/219-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V8280 PBT+PET 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | Absolute Drying; ASTM-D792 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.64 g/cc @Temperature 25.0 °C |
1.64 g/cc @Temperature 77.0 °F |
|
Dow Corning 236 DISPERSION Flowable (as supplied) silicone RTV coatingInformation provided by Dow Corning |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Specific Gravity | 1.64 g/cc | 1.64 g/cc | Part A; TM R050-16 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |