Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PE CONC 1 Polyethylene, Low Density (LDPE) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Oceanchem Group Potassium Formate 74-75% liquid Molecular Formula: KCOOHInformation Provided by Oceanchem Group |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R355AM Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Sylvin Technologies 8999-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Aquasil® "BP" 3641 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® 2750 Sparkle Silver® 2750 is a coarse, regular purity , high sparkle, non-leafing aluminum pigment popular for solvent Automotive Applications. This pigment can be used with tints to produce a wide ra.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Teknor Apex Fireguard® 910-LBF Polyvinyl Chloride, Flexible RoHS Compliant Features: Bromine Free; Flame Retardant; Low Smoke Emission Uses: Insulation; Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 556 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 751 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Tra-Con Tra-Cast 3135 Low Viscosity Encapsulant TRA-CAST 3135 is a low viscosity adhesive developed for demanding electronic underfill and encapsulant adhesive applications. This solvent free material is readily mixed, and cured at room temperatu.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Specific Gravity | 1.58 - 1.62 g/cc | 1.58 - 1.62 g/cc | ASTM D-792 |
Axiall 1280 Nat04 Plenum Flexible PVC Plenum-grade jacket for Category 5(+) applications with good low temperature properties. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Specific Gravity | 1.58 - 1.63 g/cc | 1.58 - 1.63 g/cc | ASTM D792 |
BLUESTAR PBT 403M-G30 30% Glass Filled PBT, injection molding grade, 30% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorableInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3000 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Asahi Kasei Thermylon® NSG-240A-2H 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |