Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Opaque Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D-792 |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® LGN1500 PC (Asia Pacific) |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R9788A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | Method A; ASTM D792 |
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 852-40/5-IS-RG Green PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7876-1 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 305 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL40445/2 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL40445/2 is typic.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2450E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2450E is a yellow color concentrate base in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2450E is he.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | 75°F (water = 1) |
Enviro Tech International EnSolv® n-Propyl Bromide Vapor Degreasing Solvent EnSolv is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane and other hazardous vapor degreasing and general use solvents for critical applications such as oxygen serv.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Colorite Polymers 8033 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 8644 Moldings & Extrusions Flexible PVC General purpose extrusion compound. Forms a good bond with rigid PVC in co-extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | |
BCC Products BC 5114 Epoxy Laminating System BC 5114 is a gray low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use abov.. |
|||
Specific Gravity | 1.31 - 1.35 g/cc | 1.31 - 1.35 g/cc | ASTM D-792 |
Axiall 18660 Moldings & Extrusions Flexible PVC Flame retardant extrusion and molding compound recommended for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |