Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D792 |
S&E Specialty Polymers CPE-01-266LT PVC Application: 90°C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced low temperature properties.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 898-08/175-IS-RG Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 898-10/161-IS-RG White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 42/165-RG-GE (CS) Red Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D 792 |
Karina 650D08/244-D-IS Beige PVC Compound Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 800-48/1-IS-RG Black PVC Compound PVC compound recommended for extrusion of notebook spiresInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 846-10/79-IS-RG White PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 852-39/156-IS-RG Pink PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 861-40/28-IS-RG Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 80/278-IS-RG Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 808-47/14-IS-RG Silver PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 836-10/132-IS-RG White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8642 Moldings & Extrusions Flexible PVC General purpose, fungus resistant extrusion and molding compound recommended for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 16881 Coax & Telecom Flexible PVC 90C rated, non-lead stabilized jacket compound with excellent low temperature properties. Suitable for riser and optical fiber constructions.Information provided by Georgia GulfGeorgia Gulf became .. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 17940 Wire & Cable Flexible PVC THW insulation compound. Also suitable for 105C applications in 3/64 and larger sizes. UL recognized component for THW. Oil resistant I, VW-1 rated.Information provided by Georgia GulfGeorgia Gul.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 18901 Wire & Cable Flexible PVC General purpose, non-lead stabilized, 105°C rated jacketing compound. Formulated to have good migration resistance and flame retardant properties.Information provided by Georgia GulfGeorgia Gulf b.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19930 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 22905 Coax & Telecom Flexible PVC Non-lead tray cable jacket for 75°C maximum service temperature.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 4420 Flexible PVC High speed TWP wire harness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8603 Moldings & Extrusions Flexible PVC A soft extrusion compound with rubber-like properties and oil resistance. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8742 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips, screen splines and other extruded shapes and profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8916 Moldings & Extrusions Flexible PVC A satin finish extrusion compound best suited for extruded T-moldings, tubings and other shapes where uniform flow through the die is required. The compound exhibits excellent abrasion resistance.I.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19850 Moldings & Extrusions Flexible PVC Primary insulation compound recommended for 105C, 1/32 wall and larger applications. Also well suited for plug molding. UL rated 94 HB.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 19801 Wire & Cable Flexible PVC Primary insulation and jacketing compound recommended for 105°C applications at a minimum wall of 15 mils. CSA approved AWM, SVT, SJT, ST, SVTO, SVTOO, SJTO, SJTOO, STO, STOO constructions. 60°C.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 48562 Moldings & Extrusions Flexible PVC Automotive window encapsulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 802-27/13-IS-RG Smoky Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 38602 Coax & Telecom Flexible PVC CATV and general purpose jacket with excellent low temperature properties. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 4520 Flexible PVC Non-lead stabilized, thin wall, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 8911 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound. UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |