Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Nylene® Norpex® AX20MRFR , 20% Mineral Reinforced, Flame Retardant Polyphenylene Ether Description: Norpex® AX20MRFR is a 20% mineral reinforced, flame retardant PPE. AX20MRFR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all opertin.. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D792 |
S&E Specialty Polymers G-2194 Application: Clear, UV resistant, extrusion compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D297 |
Parker Chomerics ParPHorm® L1938-45 Non-Conductive Form-in-Place Gasket A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material cost versus .. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Kolon KOPA® KN333G15SIBL G/F Reinforced Nylon 66 High strength, high toughnessApplications Relay coversInformation provided by API-Kolon. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina 722-48/1-A-IS Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Lucent Polymers TPP-340 Polypropylene, 40% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.24 - 1.30 g/cc | 1.24 - 1.30 g/cc | ASTM D 792 |
Karina E 42/261-GEN Dark Red MBATCH (SP31543) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | Original Properties; ASTM D297 |
Freudenberg Simrit N470 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D297, 15 |
Seals Eastern 7284 Butyl and Halobutyl Rubber Chlorobutyl; High damping; Non-conductiveInformation provided by Seals Eastern, Inc. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D 792 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Teknor Apex APEX® 3800-85 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | |
Shin-Etsu Silicones KE-7021U Temperature Resistant Silicone Elastomer KE7021 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 315 °C (67 ~ +600 °F)Typ.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Teknor Apex APEX® 7500-90 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | Mixed |
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Lubrizol ESTANE® 58138 Ester Based Thermoplastic Polyurethane Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | Molded; ASTM D792 |
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | catalyzed with QM CAT BLUE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® TFPP 2040 Talc Filled Polypropylene AAROPRENE® TFPP 2000 Series Talc Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
Colorite Polymers 5514 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | Mixed; TM R050-16 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
EG80A-B20 Polyurethane-based Biomedical Elastomer |