Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 2.17 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
ISO 12086
Isoflon PFA Polyperfluoroalkoxyethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and..
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and..
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D-792
Saint-Gobain Norton® FEP Fluoropolymer Film
Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
at 25°C
Daikin NEOFLON AP-210AS PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Daikin NEOFLON NP-40 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
at 25°C
Daikin NEOFLON AP-201 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
at 25°C
Daikin NEOFLON AP-210 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided ..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
at 25°C
Daikin NEOFLON AP-230 PFA Pellets
NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries.
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
ASTM D792
Adamas Adalon® 992 Modified PTFE
Information provided by Adamas, HPM
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Asahi Glass Fluon® P-66P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
ASTM D792
Adamas Adalon® 503 PTFE, 0.1% MoS2
Information provided by Adamas, HPM
Specific Gravity 2.16 - 2.17 g/cc
2.16 - 2.17 g/cc
ASTM D792
Adamas Adalon® 508 PTFE, 1% MoS2
Information provided by Adamas, HPM
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Asahi Glass Fluon® P-802UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, ..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ISO 12086
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer
Fluoropolymer material specifications.Information provided by Isoflon.
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff..