Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.00 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.960 - 1.00 g/cc
0.960 - 1.00 g/cc
ASTM D1505
S&E Specialty Polymers GPP1001V0M-HCO-15 PP
Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high lev..
Specific Gravity 0.970 - 1.00 g/cc
0.970 - 1.00 g/cc
ASTM D792
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Coating X300™ AF Waterborne coating
Description: Waterborne coating demonstrating excellent water hold outUsage: Coating X300â„¢AF provides high levels of water resistance and good moisture resistance for kraft paper. Coating X300â..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® DigiPrime® 2000 Primer
Description: Primer for digital printing Usage: DigiPrime® 2000 is flexo and gravure ready and provides excellent adhesion of Indigo inks to uncoated, mottled, semi-gloss and glossy paper grades...
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® DigiPrime® 2500 Primer
Description: Primer for digital printing suitable for paper substratesUsage: DigiPrime® 2500 is a product that can be added to size press treatments or pigment coatings to optimize substrates for..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® DigiPrime® 6029 Primer
Description: Primer for digital printingUsage: DigiPrime® 6029 is a flexo and gravure ready coating used to optimize substrates for HP Indigo printing. This product provides excellent adhesion of..
Specific Gravity 0.940 - 1.00 g/cc
0.940 - 1.00 g/cc
Michelman® Hydrosize® PA845 Anionic polyamide dispersion
Description: Anionic polyamide dispersionUsage: Hydrosize® PA845 is an APE free, aqueous nylon dispersion designed to be used as a fiber sizing in fiber reinforced nylon composites where greater ..
Specific Gravity 0.960 - 1.00 g/cc
0.960 - 1.00 g/cc
Michelman® Hydrosize® PP2-01 Nonionic polypropylene emulsion
Description: Nonionic polypropylene emulsionUsage: Hydrosize® PP2-01 is an APE-free sizing for fiberglass for LFT and carbon fiber with excellent bond strength.Application data: Small particle si..
Specific Gravity 0.990 - 1.00 g/cc
0.990 - 1.00 g/cc
Michelman® Licomer® IN 41 Anionic / Nonionic polyethylene emulsion
Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® IN 41 is a high anti-slip additive for floor polish formulations.Information provided by Michelman®
Specific Gravity 0.990 - 1.00 g/cc
0.990 - 1.00 g/cc
Michelman® Licomer® W 315 FP Anionic / Nonionic polyethylene emulsion
Description: Anionic / Nonionic polyethylene emulsionUsage: Licomer® W 315 FP is a high anti-slip emulsion suitable for floors, finishes on shoes, leather, etc.Information provided by MichelmanÂ..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 11226 Cationic polypropylene emulsion
Cationic polypropylene emulsionUsage: Michem® Emulsion 11226 is useful as an additive in fiberglass sizing formulations which are used to reinforce polypropylene. This emulsion has a very high mo..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 18325 Nonionic polyethylene wax emulsion
Description: Nonionic polyethylene wax emulsionUsage: Michem® Emulsion 18325 as an additive provides excellent water and chemical resistance in film coatings.We serve many markets through MichemÂ..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 29730 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 28640 is a used as a binder and substrate coating for fibers and composites. Michem® Emulsion 29730 protects glass during fib..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 44730 Nonionic ethylene acrylic acid copolymer
Description: Nonionic ethylene acrylic acid copolymerUsage: Michem® Emulsion 44730 as a formalin and APE free additive which provides anti-slip and black heel mark resistance. These properties ar..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 52137 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 52137 as an additive, provides lubricity and is effective as a high temperature mold release for metal dies.We serve many market..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 98040M1 Nonionic Fischer Tropsch wax emulsion
Description: Nonionic Fischer Tropsch wax emulsionUsage: Michem® Emulsion 98040M1 is an additive used to provide superior slip and antiblock properties. This product is successfully used in paint..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Flex P1883 Water based heat seal coating and primer
Description: Water based heat seal coating and primer for extrusion coated resins.Usage: Michem® Flex P1883 is a general purpose primer for metal and paper substrates to promote adhesion to extru..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Guard 1350 Nonionic emulsion of polyethylene wax
Description: Nonionic emulsion of polyethylene waxUsage: Michem® Guard 1350 is a water based one micron dispersion which improves rub and abrasion resistance in pigmented coatings and semi-gloss ..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Lube 110 Anionic carnauba/polyethylene wax emulsion
Description: Anionic carnauba/polyethylene wax emulsionUsage: Michem®Lube 110 provides superior slip as well as good antiblock and abrasion resistance in coating applications.Compatible with ingr..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Lube 182 Anionic carnauba/paraffin wax emulsion
Description: Anionic carnauba/paraffin wax emulsionUsage: Michem® Lube 182 can provide slip, release and anti-block properties in a number of applications ranging from wood coatings to being blen..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Lube 190 Anionic polyethylene wax emulsion
Description: Anionic polyethylene wax emulsionUsage: Michem® Lube 190 provides mar and scratch resistance as well as improved water resistance and is useful in the coatings and graphic arts indus..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Prime 2960 Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 2960 provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent re..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4990R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Shield 251 Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Shield 251 is an additive which provides abrasion resistance in coatings formulations. Michem® Shield 251 has proven most effective in..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® VaporCoat® 2200R MVTR
Description: MVTR, water and grease resistance coatingUsage: VaporCoat® 2200R is a coating which provides water and grease resistance and excellent MVTR properties on kraft liner and other substr..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 72040 Nonionic polyethylene wax emulsion
Description: Nonionic polyethylene wax emulsion Usage: Michem® Emulsion 72040 was designed to be an additive for the graphic arts industry and provides excellent rub, mar and scratch resistance.W..
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Michelman® Michem® Emulsion 93135M Nonionic polyethylene emulsion
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93135M is a phenol and formaldehyde free wax emulsion used in floor polish formulations for black heel mark resistance, toughnes..
Specific Gravity 0.960 - 1.00 g/cc

@Temperature 25.0 °C
0.960 - 1.00 g/cc

@Temperature 77.0 °F
Dow Corning 3-4237 DIELECTRIC FIRM GEL KIT
Two-part, translucent green, heat cure, firm, long working time, primerless chemical adhesion.Information provided by Dow Corning
Specific Gravity 0.930 - 1.00 g/cc
0.930 - 1.00 g/cc
ASTM D792
Buckeye Polymers BP FLEX D4107 C BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Specific Gravity 0.960 - 1.00 g/cc
0.960 - 1.00 g/cc
ASTM D792
S&E Specialty Polymers GPP1001V0M-HCO PP
Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications.  It affords medium impact resistance with a high level of flam..