Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Emulsion 93135M Nonionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 93135M Nonionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93135M is a phenol and formaldehyde free wax emulsion used in floor polish formulations for black heel mark resistance, toughness and buffability, and mar, scuff and chemical resistance.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamFood Contact Information when manufactured in the USA: FDA:176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 64.5 - 65.5 %
64.5 - 65.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
9.5 - 11
9.5 - 11
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Tan, translucent liquid
Emulsifier Charge Nonionic
Solids Type High Density Polyethylene
Users viewing this material also viewed the following: