Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.10 - 2.20 g/cc | 2.10 - 2.20 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Specific Gravity | 2.10 - 2.20 g/cc | 2.10 - 2.20 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | Wet; ASTM D1475 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | Wet; ASTM D1475 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | |
Reade Advanced Materials Diatomite Powder Description: Diatomite is a sedimentary rock, white to light yellow in color, composed of the fossilized skeletons of diatoms, one celled algae-like plants which accumulated in marine or lacustrine .. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | ASTM D792 |
Rogers Corporation RO3730 Antenna Grade Laminate RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of.. |
|||
Specific Gravity | 2.10 - 2.30 g/cc | 2.10 - 2.30 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | |
Resin Technology Group TIGA 951 One-Part Silver Conductive Epoxy System Cure 10 minutes at 120°CTIGA 951 is an electrically conductive, silver-filled epoxy adhesive recommended for electronic bonding and sealing applications. This one-part, smooth paste formulation of .. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | -40°C for 1,000 hrs; JIS-K-6220; ASTM D 792 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | -40°C for 30 min and 125°C for 30 min. for 1,000 times; JIS-K-6220; ASTM D 792 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | 80°C for 1,000 hrs; JIS-K-6220; ASTM D 792 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | STM 2 |
Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easil.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | Mixed |
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | Cured |
Tra-Con Tra-Bond 933-1 Moisture Resistant Chip Encapsulant TRA-BOND 933-1 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | Mixed |
Tra-Con Tra-Bond GA47-2LV Instrument Adhesive TRA-BOND GA47-2LV low viscosity adhesive is designed for guidance instrument applications. This adhesive exhibits excellent compatibility with conventional gyro flotation fluids. TRA-BOND GA47-2LV a.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | Mixed |
Tra-Con Tra-Bond 813J01 Silicone Encapsulant TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | ASTM-D792 |
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Specific Gravity | 2.10 - 2.14 g/cc | 2.10 - 2.14 g/cc | ASTM D792 |
Daikin NEOFLON M-300H PCTFE Granular Molding Powder NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by.. |
|||
Specific Gravity | 2.10 - 2.14 g/cc | 2.10 - 2.14 g/cc | ASTM D792 |
Daikin NEOFLON M-400H PCTFE Granular Molding Powder NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process.. |
|||
Specific Gravity | 2.10 g/cc @Temperature 25.0 °C |
2.10 g/cc @Temperature 77.0 °F |
|
Dow Corning 340 Heat Sink Compound White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |
|||
Specific Gravity | 2.10 - 2.12 g/cc | 2.10 - 2.12 g/cc | ASTM D792 |
Asahi Glass Fluon® P-810UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | |
3M Dyneon™ 301Z Translucent Perfluoroelastomer System Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica.. |
|||
Specific Gravity | 2.10 g/cc | 2.10 g/cc | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Specific Gravity | 2.10 - 2.16 g/cc | 2.10 - 2.16 g/cc | ISO 12086 |
Isoflon PCTFE Polychlorotrifluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |