Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.88 g/cc | 1.88 g/cc | |
Omya OMYAFLOW® F - SY Calcium Carbonate A high purity, fine, wet ground natural calcium carbonate available in slurry form.Applications: Decorative paints.Information supplied by Omya North America. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | |
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM D792 |
PolyOne Edgetek® SF-35GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedUL 94 V0 (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 522 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM 792 |
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM D297, 15 |
Seals Eastern 7040 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM D297, 15 |
Seals Eastern 5795 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | |
BYK Cloisite® 93A Nanoclay Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | |
3M Dyneon™ FPO 3740 Fluoroelastomer 3M™ Dyneon™ FPO 3740 is a peroxide curable fluoroelastomer terpolymer containing 69.5 wt% fluorine. FPO 3740 can be used in compression, transfer or injection molding, and extrusion processes. Fea.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM D792 |
Cheng Yu Plastic E2350 Flame Retardant PET, 50% Glass Fiber |
|||
Specific Gravity | 1.88 - 1.94 g/cc | 1.88 - 1.94 g/cc | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Specific Gravity | 1.88 - 1.96 g/cc | 1.88 - 1.96 g/cc | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Specific Gravity | 1.88 - 1.92 g/cc | 1.88 - 1.92 g/cc | |
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Specific Gravity | 1.88 - 1.92 g/cc | 1.88 - 1.92 g/cc | molded |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Specific Gravity | 1.88 g/cc | 1.88 g/cc | ASTM D792 |
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |