Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | |
Oceanchem Group Melamine Cyanurate (MCA) Molecular Formula: C6H9N9O3Cas No.: 37640-57-6Physical Appearance: Fine, white, crystalline powder, nontoxic, odorless; indissolvable in water and most organic solvents.Use: Melamine Cyanurate is a .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 - 2.20 g/cc | 1.70 - 2.20 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | |
Lord Adhesives Thermosetâ„¢ ME-525 Underfill Encapsulant LORD Thermosetâ„¢ ME-525 encapsulant is a high purity, semiconductor grade epoxy underfill product developed for the encapsulation of flip chip devices. It is formulated to reduce warpage and wit.. |
|||
Specific Gravity | 1.70 - 1.76 g/cc | 1.70 - 1.76 g/cc | NBR NM-IEC 60511-1-3 |
Karina 10/1-FC-LMP (SDB) White Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D-792 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | |
Shin-Etsu Silicones FE-281U Fluorosilicone Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | Mixed |
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required.. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | Dow Method |
Dow Saran® 168 Information provided by Dow |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | silicone property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | |
Aremco Aremco-Bond™ 2220 High Performance Epoxide Ceramic-Filled, High Chemical Resistance, Machinable. For Repairing Deeply-Corroded Parts. |