Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Method A; ASTM D792 |
LNP Thermocomp® OF-1006 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R355AM Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
PolyOne Edgetek® NL-30GF/000 FR Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
KYDEX® 6200 LTR Thermoforming Sheet for Mass Transit Applications Features:Specifically designed for mass transit industriesCompliant with SMP800CMeets flamespread and smoke density requirements for mass transitExcellent formability and fabrication qualityGood def.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SPS Guang Zhou POBUXâ„¢ 3001EPG30 Non-halogen flame retardance/GF30%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® 3641 Sparkle Silver® 3641 is a coarse, regular purity, non-leafing aluminum pigment. It is characterized by high sparkle, a white face color and deep flop. An acid resistant purity version, Sparkle Si.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 353 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 354 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 303AR Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Silberline Sparkle Silver® Premier 552 Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
Tra-Con Tra-Cast 3135 Low Viscosity Encapsulant TRA-CAST 3135 is a low viscosity adhesive developed for demanding electronic underfill and encapsulant adhesive applications. This solvent free material is readily mixed, and cured at room temperatu.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | |
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Specific Gravity | 1.58 - 1.63 g/cc | 1.58 - 1.63 g/cc | ASTM D792 |
BLUESTAR PBT 403M-G30 30% Glass Filled PBT, injection molding grade, 30% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorableInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | Method A; ASTM D792 |
LNP Thermocomp® JF-1006 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Specific Gravity | 1.58 g/cc | 1.58 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 530HTE NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate with Excellent High Temperature Dielectric PropertiesRynite 530HTE NC010 is a 30% glass reinforced modified polyethylene terephthalate resin with exce.. |